NEWS

Why Chip Resistors Fail in Pulp Mills in Finland: Metsä Fibre Upgrades the Kemi Mill and 7,926 Walsin Anti-Sulfur Parts in 0603

Standard thick film chip resistors fail in pulp mills because sulfur gases reach the silver inside the terminations and turn it into silver sulfide, which does not conduct, until the part reads open. An anti-sulfur chip resistor changes that inner layer. Walsin lists 7,926 anti-sulfur parts in 0603 alone. Venatech is the authorised Walsin distributor in Hong Kong.


Venatech Limited, an authorised Walsin Technology (Walsin) distributor in Hong Kong, wrote this engineering note for Finnish designers and buyers of electronics that live inside pulp, paper and chemical plants: drives, distributed control I/O, analysers, valve positioners and instrumentation. We counted every Walsin figure on 21 November 2026 across our 79 chip resistor upload files, Venatech_ChipR_Upload_01.xlsx to Venatech_ChipR_Upload_79.xlsx, and checked each part against our ready stock snapshot dated 9 November 2026. The one test reference below comes from a Stackpole datasheet on seielect.com, fetched the same day; Stackpole is a line we supply.

What is Metsä Fibre changing at the Kemi mill in 2026?

Its cooking system. Andritz announced on 12 May 2026 that it will convert the cooking system at Metsä Fibre’s Kemi bioproduct mill to single-vessel continuous cooking, with start-up scheduled for the fourth quarter of 2026 and capacity of about one and a half million tonnes of pulp a year after the upgrade.

The Andritz scope also includes a new chip feeding system and a vapor reboiler, which the company says will improve digester heat recovery and reduce odorous gas emissions. Those are Andritz’s statements, not ours, and we make no claim about the mill’s electronics or who supplies them. We use Kemi because it is a 2026 reminder of what a Finnish kraft mill is: a large, continuous chemical process in which reduced sulfur gases are part of the chemistry, and in which control cabinets, drives and field instruments run for years in that air.

Why do standard chip resistors fail in pulp mills?

Because of silver sulfide. A standard thick film chip has a silver-bearing inner termination under its nickel and tin layers; sulfur gases such as hydrogen sulfide creep in at the edge of the protective coat, react with the silver and grow silver sulfide, raising resistance until the part goes open.

The failure is slow and quiet. A board can pass every factory test and work for a year or two in a mill before resistance on the worst-exposed parts starts to climb, first on high-value pull-ups and dividers where a few percent shift goes unnoticed, then to an open circuit. Heat and humidity speed it up, and so does any gap in conformal coating at the chip’s ends. Kraft pulping is a textbook sulfur environment, and rubber processing, waste water treatment, geothermal sites and some mining operations behave the same way. The fix in the part is an inner termination that does not contain exposed silver, or a structure that keeps sulfur away from it; the fix around the part is coating, sealing and filtered cabinet air. Both are worth having. Our earlier note on anti-sulfuration resistor counts takes the data view of the same families.

How is an anti-sulfur chip resistor tested?

By exposing it to sulfur for hundreds of hours and measuring the shift. Stackpole’s RMCS datasheet, fetched 21 November 2026, lists 1,000 hours in hydrogen sulfide at 50 C and 91 to 93 percent relative humidity, with no power applied, and a limit of plus or minus 0.5 percent plus 0.05 ohm; it cites ASTM B809-95 alongside.

ASTM B809 is the flowers of sulfur test, in which parts sit in a closed vessel above elemental sulfur at elevated temperature and humidity. The two methods are not interchangeable, so the useful question to put to any supplier is which test, how many hours, at what temperature, and what shift was allowed. Datasheets differ on all four. When you compare an anti-sulfur part from one maker with another, line those four values up before you compare part numbers.

Check the datasheet. Our Walsin export labels parts as anti-sulfuration but does not state the test method, duration or pass limit. Read those on the Walsin datasheet for the family you choose, and compare them with the limit in your own environmental specification.

How many Walsin anti-sulfur chip resistors are there?

41,147 in all, 7,926 of them in 0603. We counted 41,147 distinct Walsin chip resistors labelled anti-sulfuration across eight series, from 0201 to 2512; 23,530 of them are also labelled AEC-Q200, and 0603 is the deepest size with 7,926 parts at 800 resistance values.

Walsin anti-sulfur series Distinct parts In 0603
High grade anti-sulfuration, automotive 12,871 1,799
General purpose anti-sulfuration, automotive 10,659 1,938
High power, anti-sulfuration 9,135 1,661
High precision, anti-sulfuration 5,710 1,142
Arrays, four series (two and four element) 2,772 1,386
All anti-sulfur 41,147 7,926

We have not seen the 0603 cut published elsewhere. Of the 7,926 parts in 0603, 3,737 are labelled AEC-Q200, which many industrial buyers now ask for as a quality floor even outside vehicles. These parts are quoted through our authorised Walsin channel.

Which Walsin 10 kOhm 0603 parts replace a standard chip in a mill?

Six anti-sulfur options cover the usual jobs. At 10 kOhm in 0603, Walsin offers anti-sulfur parts in general purpose, high grade, high power, precision and array forms, so a standard 1 percent chip can be swapped like for like without changing the footprint.

Walsin part, 10 kOhm, 0603 What the export states Use in a mill board Match / mismatch vs a standard 1 percent chip Your incumbent
WR06X1002FTL General purpose, 1 percent, 100 ppm, not anti-sulfur The part being replaced Mismatch sulfur resistance
WR06X1002FTLV General purpose anti-sulfur, AEC-Q200, 1 percent, 100 ppm Pull-ups, bias, logic Match size, value, tolerance, TCR
SR06X1002FTL High grade anti-sulfur, AEC-Q200, 1 percent, 100 ppm Long-life control and I/O boards Match size, value, tolerance, TCR
SF06P1002FTP High power anti-sulfur, 1 percent, 100 ppm, 0.125 W Warmer spots, drive boards Match size, value; power higher
SF06H1002BTL Precision anti-sulfur, 0.1 percent, 100 ppm Analog front ends, dividers Match size, value; tolerance tighter
SA06X1002FTL Anti-sulfur array, four elements, 1 percent, 200 ppm Bus pull-ups in one part Footprint differs; TCR wider

Have part numbers to quote? Click any Walsin part number in the table to open its page and add it to your RFQ, or upload your BOM for a quote, or cross your current part in VenaMatch. E-mail sales@venatech.com.hk or call (852) 2628 4777. We confirm availability, date code and lead time on each quote.

For a mill, start with the high grade or general purpose anti-sulfur part for anything digital, and the precision anti-sulfur part for any resistor whose drift would move a reading. Keep the board coating, because no anti-sulfur termination protects a solder joint or a copper trace.

How Venatech helps

Swap the risk, not the layout. Venatech is the authorised Walsin distributor in Hong Kong; VenaMatch decodes part numbers from 18 manufacturers and crosses 800,000+ parts to Walsin, so a list of standard chips comes back with anti-sulfur alternatives in the same size and value.

Paste your resistor lines into the cross-reference tool, or upload the full parts list at BOM upload; ready stock shows the lines we hold in Hong Kong (snapshot 9 Nov 2026). For the anti-sulfur parts above, request a quote and we source them through our authorised Walsin channel. We serve Finnish buyers from Hong Kong in small lots and confirm availability, date code and lead time on each quote, with no price, lead-time or stock guarantee. The chip resistor range lists every Walsin family.

The short version

  • Andritz will rebuild the cooking system at Metsä Fibre’s Kemi mill for start-up in the fourth quarter of 2026, per its 12 May 2026 release, including a vapor reboiler to cut odorous gas emissions.
  • Standard thick film chips fail in sulfur air when silver in the inner termination turns to silver sulfide.
  • Walsin lists 41,147 anti-sulfur chip resistors, 7,926 in 0603, and 23,530 labelled AEC-Q200.
  • Compare test method, hours, temperature and pass limit on the datasheets, and keep the board coating.

Send us the resistor lines from a board that lives in a mill, and we will return anti-sulfur Walsin alternatives with every difference stated. Have you seen open resistors come back from the field?

Related reading

Last reviewed: 21 November 2026.

Sources

Fetched 21 November 2026.

  • Andritz newsroom, release on the Metsä Fibre Kemi cooking system upgrade, 12 May 2026: https://www.andritz.com/newsroom-en/pulp-paper/2026-05-12-mf-kemi-cooking-group
  • Stackpole Electronics RMCS datasheet (SEI-RMCS.pdf), sulfur test conditions: https://www.seielect.com/catalog/SEI-RMCS.pdf
  • Venatech Walsin chip resistor upload files (Venatech_ChipR_Upload_01.xlsx to Venatech_ChipR_Upload_79.xlsx) and ready stock snapshot dated 9 November 2026, re-measured 21 November 2026.

Frequently asked questions

Why do chip resistors fail in pulp mills in Finland?

Sulfur gases from the kraft process reach the silver in a standard chip’s inner termination and form silver sulfide, which does not conduct. Resistance rises over months until the part reads open.

What is an anti-sulfur chip resistor?

A chip resistor whose inner termination is built so that sulfur cannot reach or attack the silver. It keeps the same size and value as a standard chip, so it drops into the same footprint.

How many Walsin anti-sulfur chip resistors are there?

41,147 in our chip resistor files across eight series, 7,926 of them in 0603, and 23,530 also labelled AEC-Q200.

Which Walsin part replaces a standard 10 kOhm 0603 resistor in a sulfur atmosphere?

WR06X1002FTLV or SR06X1002FTL, both anti-sulfur, AEC-Q200, 1 percent and 100 ppm, match a standard 1 percent 10 kOhm 0603 on size, value, tolerance and TCR.

Is conformal coating enough on its own?

Not reliably. Sulfur reaches the chip ends through thin or missing coating at the terminations; anti-sulfur parts and good coating together give the best margin.

How is sulfur resistance tested?

By sulfur exposure for hundreds of hours: one Stackpole datasheet lists 1,000 hours in hydrogen sulfide at 50 C, and ASTM B809 describes a flowers of sulfur test. Compare method, hours, temperature and pass limit.


Share This, Choose Your Platform!