Thin film vs thick film resistor noise comes down to about 30 dB. A standard thick-film resistor runs near minus 10 dB of current noise, thin film near minus 30 to minus 40 dB. With 2.5 V across a 10 kOhm part, that is about 1.4 microvolts against 0.14. Venatech is the authorised Walsin distributor in Hong Kong.
Venatech Limited, an authorised Walsin distributor in Hong Kong, wrote this for analog and sensor engineers in Auckland, Christchurch and across New Zealand who design patient monitors, respiratory devices, flow and pressure sensors and other low-signal front ends, and for the buyers who source their resistors. Walsin Technology (Walsin) is the line we are authorised for. On 18 November 2026 we parsed our six thin-film upload files, Venatech_ThinFilm_WF.xlsx, _WFQ.xlsx, _SF.xlsx, _SFA.xlsx, _SFQ.xlsx and _MF.xlsx, 1,168,998 distinct part numbers, and our 79 chip resistor upload files, filtered both to exactly 10 kOhm in 0603, and checked the result against our ready stock snapshot dated 9 November 2026. Every part number below is real.
Why does New Zealand’s medical device industry ask about resistor noise?
Because its products measure small signals, and the sector is growing. Fisher and Paykel Healthcare reported in its release of 26 May 2026 that operating revenue for the 2026 financial year rose 14 percent to 2.31 billion New Zealand dollars, and that it progressed construction of a fifth building on its East Tamaki campus in Auckland, adding manufacturing and product development space.
Those are the company’s figures, not ours, and we make no claim about which components it or any other maker uses. What the release describes is a medical technology base in New Zealand that designs and builds electronics close to home. Sensor and patient-signal circuits share one trait: the wanted signal can be microvolts, so every source of noise in the front end is part of the error budget. Resistors add two kinds, thermal noise, which every resistor has, and excess or current noise, which depends heavily on how the resistor is made.
Thin film vs thick film resistor noise: how big is the difference in microvolts?
Roughly ten times. With 2.5 V DC across a 10 kOhm resistor over 0.1 to 100 Hz, three decades, a thick-film part at minus 10 dB adds about 1.37 microvolts rms of excess noise, and at minus 3 dB about 3.07; a thin-film part at minus 30 dB adds about 0.14 and at minus 40 dB about 0.04.
The noise-index ranges come from Passive Components Blog’s resistor noise article, updated 6 August 2026: minus 10 to minus 3 dB for standard thick film, minus 20 to minus 10 dB for improved low-noise thick film, and minus 30 to minus 40 dB for thin and metal film. We converted dB to microvolts per volt per decade by the usual definition, 0 dB equal to 1 microvolt per volt, and multiplied by the voltage and the square root of the number of decades.
| 10 kOhm, 2.5 V DC across, 0.1 to 100 Hz | Noise index | Excess noise, rms | Ratio to thermal noise, 0.13 microvolt | Fit for a 0.5 microvolt front-end budget |
|---|---|---|---|---|
| Thick film, standard, noisy end | minus 3 dB | 3.07 microvolts | about 24x | Mismatch |
| Thick film, standard | minus 10 dB | 1.37 microvolts | about 11x | Mismatch |
| Thick film, low-noise grade | minus 20 dB | 0.43 microvolts | about 3x | Match, little margin |
| Thin film | minus 30 dB | 0.14 microvolts | about 1x | Match |
| Thin film, quiet end | minus 40 dB | 0.04 microvolts | about 0.3x | Match |
The thermal figure is the 4kTR noise of 10 kOhm at 27 C, 12.9 nanovolts per root hertz, over a 100 Hz bandwidth. Check the datasheet: the noise index is not in Walsin’s parametric export, and a typical range from an article is not a guarantee for any one part.
When does resistor excess noise matter, and when can you ignore it?
Only when DC voltage sits across the resistor. Excess noise scales with the DC voltage across the part: a 10 kOhm feedback resistor with no DC across it adds only its 12.9 nanovolts per root hertz of thermal noise, whatever its construction, while the same value in a bridge, a bias divider or a reference string adds excess noise in proportion to its volts.
So the choice is position by position. In an AC-coupled biopotential gain stage, thick film is often fine. In a sensor bridge excited at 2.5 or 5 V, a reference divider feeding an ADC, or a transimpedance stage with DC on the output, thin film usually earns its place, and it also brings tighter TCR. Our post thin film versus thick film chip resistors covers construction, and thick film versus thin film precision resistor TCR crossover covers drift. Excess noise is also mostly 1/f noise, so it matters most in low-frequency work like ECG, respiration and pressure sensing.
Which Walsin 10 kOhm 0603 resistors fit a low-noise front end?
The thin-film WF parts, from 3 ppm up. For a 10 kOhm, 0603, 25 ppm or better, low-noise bridge brief, the WF precision thin-film parts below match; the thick-film parts, even at 25 ppm and 0.1 percent, miss on construction, because their noise index belongs to thick film.
| Brief: 10 kOhm, 0603, DC across, low noise, 25 ppm or better | Walsin part | Construction, series | Tolerance | TCR | Power | Match / mismatch |
|---|---|---|---|---|---|---|
| Lowest drift | WF06B1002TTL |
Thin film, WF precision | 0.01% | 3 ppm | 1/10 W | Match |
| Very low drift | WF06Z1002TTL |
Thin film, WF precision | 0.01% | 5 ppm | 1/10 W | Match |
| 25 ppm thin film | WF06R1002TTL |
Thin film, WF precision | 0.01% | 25 ppm | 1/10 W | Match |
| 25 ppm, lower power | WF06U1002TTL |
Thin film, WF precision | 0.01% | 25 ppm | 1/16 W | Match where dissipation is low |
| Thick film, 25 ppm | WF06J1002BTL |
Thick film, high precision TC25 | 0.1% | 25 ppm | 1/10 W | Mismatch on noise construction |
| Thick film, 50 ppm | WF06K1002BTL |
Thick film, high precision TC50 | 0.1% | 50 ppm | 1/10 W | Mismatch on noise and TCR |
| General purpose | WR06X1002FTL |
Thick film, general purpose | 1% | 100 ppm | 1/10 W | Mismatch; fine where no DC sits across it |
Have part numbers to quote? Click any Walsin part number in the table to open its page and add it to your RFQ, or upload your BOM for a quote, or cross your current part in VenaMatch. E-mail sales@venatech.com.hk or call (852) 2628 4777. We confirm availability, date code and lead time on each quote.
We checked every field above against the export rows in Venatech_ThinFilm_WF.xlsx and, for the thick-film parts, Venatech_ChipR_Upload_28.xlsx and _66.xlsx, and read the construction from Walsin’s datasheet links in each row. The WF values above are the 0.01 percent grade; the same values come at 0.02 to 1 percent in the thin-film files, so a 0.1 percent brief does not need to pay for 0.01. WR06X1002FTL is on our shelf in Hong Kong (snapshot 9 Nov 2026), and so is one 0402 thin-film 10 kOhm line at 0.1 percent and 25 ppm; the 0603 thin-film parts are to order, quoted through our authorised Walsin channel. The thin film range page lists every series.
How many Walsin 10 kOhm 0603 thin-film parts are there, by series?
176, across six series. We counted 176 distinct Walsin thin-film part numbers at exactly 10 kOhm in 0603: 56 in WF precision, 30 in WF.Q tagged AEC-Q200, 35 in SF.Q, 25 in SF.A, 10 in SF and 20 in MF tantalum nitride, with TCR from 3 to 50 ppm and tolerance from 0.01 to 1 percent.
| 10 kOhm 0603 thin-film series | Export file | Part numbers | TCR grades offered | Tightest tolerance | Fit |
|---|---|---|---|---|---|
| WF precision | Venatech_ThinFilm_WF.xlsx | 56 | 3, 5, 10, 15, 25, 50 ppm | 0.01% | Match, widest choice |
| WF.Q, AEC-Q200 | Venatech_ThinFilm_WFQ.xlsx | 30 | 5 to 50 ppm | 0.02% | Match for automotive-grade lines |
| SF.Q, anti-sulfuration, AEC-Q200 | Venatech_ThinFilm_SFQ.xlsx | 35 | 5 to 50 ppm | 0.05% | Match where sulfur exposure is a risk |
| SF.A, anti-sulfuration | Venatech_ThinFilm_SFA.xlsx | 25 | 5, 25, 50 ppm | 0.05% | Match |
| SF, anti-sulfuration | Venatech_ThinFilm_SF.xlsx | 10 | 25, 50 ppm | 0.05% | Match at 25 ppm |
| MF, tantalum nitride | Venatech_ThinFilm_MF.xlsx | 20 | 10 to 50 ppm | 0.05% | Match; moisture-resistant film |
Against that, our chip resistor export holds 95 thick-film part numbers at 10 kOhm in 0603, 20 of them high-precision. We have not seen the 10 kOhm 0603 thin-film choice counted by series and TCR anywhere else. For a medical-device documentation view, see passives for a medical device.
How Venatech helps: what can a New Zealand medical electronics team send us?
Your front-end resistor list, marked by which positions carry DC. Venatech is the authorised Walsin distributor in Hong Kong; VenaMatch decodes part numbers from 18 manufacturers and crosses 800,000+ parts to Walsin, including thick-film and thin-film chip resistors.
Paste your resistor lines into the cross-reference tool, upload the BOM at /bom/, or check the dated ready stock list. We serve New Zealand from Hong Kong in small lots, which suits samples, verification builds and low-volume medical production, and we quote fast: request a quote through the site. We confirm availability, date code and lead time on each quote and promise none in advance. Medical-device qualification and regulatory files stay with your engineers; import questions go to your compliance team.
The short version
- Fisher and Paykel Healthcare reported FY2026 operating revenue up 14 percent to 2.31 billion New Zealand dollars and a fifth building under way at East Tamaki (release of 26 May 2026).
- Thin film vs thick film resistor noise: about minus 30 to minus 40 dB against minus 10 to minus 3 dB, roughly 1.4 microvolts against 0.14 for a 10 kOhm part with 2.5 V across.
- Excess noise only matters where DC sits across the resistor; elsewhere thermal noise dominates.
- Walsin lists 176 thin-film 10 kOhm 0603 parts in six series, from 3 ppm and 0.01 percent.
Send us the bridge, divider and feedback resistors from your front end and we will return the Walsin thin-film crosses with every field stated. Which of your resistors actually has DC across it?
Related reading
- Thin film versus thick film chip resistors
- Thick film versus thin film precision resistor TCR crossover
- Passives for a medical device
- Cross-reference tool, BOM upload and ready stock snapshot
Last reviewed: 18 November 2026.
Sources
Fetched 18 November 2026.
- Fisher and Paykel Healthcare, FPH reports strong revenue and profit growth for FY26, NZX announcement of 25 May 2026, release dated 26 May 2026: https://www.nzx.com/announcements/473285
- Passive Components Blog, Resistors Noise and Corrosion, updated 6 August 2026: https://passive-components.eu/resistors-noise-and-corrosion/
- Venatech thin-film upload files (WF, WF.Q, SF, SF.A, SF.Q, MF) and chip resistor upload files Venatech_ChipR_Upload_01.xlsx to _79.xlsx, re-measured 18 November 2026; Venatech ready stock snapshot dated 9 November 2026.
Frequently asked questions
Is thin film quieter than thick film?
Typically yes, by about 20 to 30 dB of current noise: minus 30 to minus 40 dB for thin film against minus 10 to minus 3 dB for standard thick film, per the article we cite. Check each datasheet.
How do I calculate resistor excess noise?
Convert the noise index to microvolts per volt per decade, multiply by the DC volts across the part and by the square root of the decades. At minus 10 dB, 2.5 V and three decades, that is about 1.37 microvolts.
Does a feedback resistor need to be thin film for low noise?
Not for excess noise if no DC sits across it; only thermal noise remains. Thin film may still be chosen for TCR and tolerance.
Which Walsin 10 kOhm 0603 thin-film resistor has the lowest TCR?
WF06B1002TTL, at 3 ppm and 0.01 percent. The same value comes at 0.02 to 1 percent in the WF series.
Are there AEC-Q200 thin-film 10 kOhm 0603 parts?
Yes: 30 in WF.Q and 35 in SF.Q in our count of 18 November 2026. AEC-Q200 is compliant, not certified; ask for the qualification report.
Can Venatech supply thin-film resistors to New Zealand?
Yes. Venatech is the authorised Walsin distributor in Hong Kong and quotes small lots to New Zealand; one 10 kOhm thick-film 0603 line and one 0402 thin-film line are on our shelf in Hong Kong (snapshot 9 Nov 2026).